DC FieldValueLanguage
dc.contributor.authorAmirkhanlou, S-
dc.contributor.authorJi, S-
dc.contributor.authorZhang, Y-
dc.contributor.authorWatson, D-
dc.contributor.authorFan, Z-
dc.date.accessioned2016-12-14T14:34:48Z-
dc.date.available2016-10-04-
dc.date.available2016-12-14T14:34:48Z-
dc.date.issued2016-
dc.identifier.citationJournal of Alloys and Compounds, 694: pp. 313 - 324, (2016)en_US
dc.identifier.issn0925-8388-
dc.identifier.urihttp://bura.brunel.ac.uk/handle/2438/13638-
dc.description.abstractAs an intrinsic materials property and an important criterion in structural design, the Young’s modulus of cast aluminium alloys can be significantly increased through adding Si and Cu elements as well as in-situ forming Mg2Si and TiB2 particles in the alloys to make castings with complex geometry. The microstructural evaluation and mechanical properties of Al-Si-Mg alloy and Al-Si-Mg-Cu/Mg2Si-TiB2 hybrid composite were examined by X-ray diffractometer (XRD), optical microscopy (OM), scanning and high resolution transmission electron microscopes (SEM and HRTEM), ultrasonic pulse technique and tensile test. The results revealed that the Al-Si-Mg-Cu/Mg2Si-TiB2 hybrid nanocomposite could provide the Young’s modulus more than 94 GPa and the yield strength up to 235 MPa by forming the α-Al (Cu, Mg), Si, Mg2Si and TiB2 phases in the microstructure. Micromechanics-based models were also employed to explain important factors in Young’s modulus and yield strength. The theoretical calculation confirmed that the contribution of thermal mismatch, Orowan, elastic mismatch, load bearing and grain boundary strengthening mechanisms to the yield strength are 65.5, 38.3, 26.2, 6.7 and 1.4 MPa, respectively. The Al-Si-Mg-Cu/Mg2Si-TiB2 hybrid composite showed a homogeneous distribution of strengthening phases throughout the aluminium matrix, and a microstructure without any detrimental phases. The interfaces between the aluminium matrix and the TiB2 particles are clean, smooth and well-bonded. TiB2 particles tend to have hexagonal and cubic prism shapes with chamfered edges and corners due to the specific growth rate of facets.en_US
dc.description.sponsorshipFinancial support from Jaguar Range Rover (JLR) [grant number R33232] is gratefully acknowledged.en_US
dc.format.extent313 - 324-
dc.language.isoenen_US
dc.publisherElsevieren_US
dc.subjectA. Metal matrix compositesen_US
dc.subjectB. Liquid-solid reactionsen_US
dc.subjectC. Elasticityen_US
dc.subjectC. Microstructureen_US
dc.subjectC. Mechanical propertiesen_US
dc.subjectD. Transmission electron microscopyen_US
dc.subjectTEMen_US
dc.titleHigh modulus Al[sbnd]Si[sbnd]Mg[sbnd]Cu/Mg<inf>2</inf>Si[sbnd]TiB<inf>2</inf>hybrid nanocomposite: Microstructural characteristics and micromechanics-based analysisen_US
dc.typeArticleen_US
dc.identifier.doihttp://dx.doi.org/10.1016/j.jallcom.2016.10.016-
dc.relation.isPartOfJournal of Alloys and Compounds-
pubs.publication-statusPublished-
pubs.volume694-
Appears in Collections:Dept of Electronic and Electrical Engineering Research Papers